procedure of aggregate crushing value – Euromecc Aggregate Crushing Value – Civil Engineering Procedure to determine Aggregate Crushing Value i The aggregates passing through 125mm and retained on 10mm IS Sieve are ovendried at a temperature of 100 to 110 o C for 3 to 4hrs